We use West system 6/10 in a tube. Basicly it's a caulk tube with 2 chambers in it. one chamber has 105 resin & the other has 206 fast hardner. The tip of the caulk tube is about 6 inches long & has a mixing chamber, so when it comes out the very tip its mixed together. Pretty cool stuff.
Follow up with gel coat patch on the top.